Items Technopanel & Egy Bond ACP INTERNATIONAL ACP

1. Materials specifications   (1) Composition
    Skin
    Core

(1) Product tolerance
    Width
    Lenght

    Bow

    Squareness


0.5 mm aluminum sheet (3105-H14)
Low density polyethylene

±2.0mm
±3.0mm
±0.2mm
±0.3mm
maximum 0.5% of length and /or width

Maximum 5.0mm


0.5 mm t aluminum sheets (3105-H14)
Low density polyethylene

±2.0mm
±4.0mm
±0.2mm for 3mm and 4mm thick
±0.3mm for 6mm thick
Maximum 0.5% of length and /or width

Maximum 5.0mm

2. Physical Properties
(1) Panel weight
(2)Thermal expansion

Yield strenght
(ASTM E8)

Modules of temperature
(ASTM c393)

(3) Deflection temperature
(ASTM D648)

4mm
5.51 kg / m²
1.2mm / m / 50 ºC

15.kg / mm²


7000 kg / mm²


≥115 ºC

3mm            4mm           6mm
4.6 kg/m²     5.5kg/m²    7.4kg/m²
1.2mm / m / 50 ºC

15.kg / mm²


7000 kg / mm²


115 ºC

4. Fire code acceptance




5. Paint finishes
    Paint resin
    Coating line
    Solid color
    Metallic color
    Stone Series

[ United Kingdom ]
BS476 Part 7 : Class 1






Two - coat two bake / 29 µ min.
Three - coat three bake 34 µ min.
Image transfer process 39 µ min.

[ United Kingdom ]
BS476 Part 5 : Class P
Part 6 : Class O
Part 7 : Class I


Lumiflon - based fluorocarbon
Manufacturer's continuos coating line
Two - coat two bake / 29 µ min.
Three - coat three bake / 35 µ min.
Image transfer process / 45 µ min.

6. Welding of core material

7. Impact Resistance

Applicable

No Picking off after reverse impact
cross-hatch

Applicable

No Picking off after reverse impact
cross-hatch